Alloy 1.4000 Technical Data Sheet:

General information:

Alloy: 1.4000

Trade names: X6Cr13, AISI 403
Material number: 1.4000
DIN standard: X6Cr13
UNS number: S40300

Chemical composition:

Carbon content (C): 0.08% max.
Silicon content (Si): 1.00% max.
Manganese (Mn): 1.00% max.
Phosphorus (P): 0.04% max.
Sulfur (S): 0.03% max.
Chromium (Cr): 12.50–14.50%
Nickel (Ni): 0.75% max.

Physical properties:Density: 7.70 g/cm³
Melting point: 1450–1530°C
Thermal conductivity: 25 W/(m·K)
Electrical conductivity: 0.24 Ωmm²/m
Specific electrical resistance: 0.40 μΩm

Mechanical properties:

Tensile strength: 450–750 N/mm²
Yield strength: 275–485 N/mm²
Elongation at break: 15–25%
Hardness: 170–220 HB

Heat treatment:

Hardenability: by quenching and tempering at temperatures between 950 and 1050°C
Tempering hardness: at 600–700°C for an optimal combination of hardness and toughness

Applications:

Pump and valve construction
Valve and tank construction
Food industry, e.g. for knives
Chemical industry
General mechanical engineering